• Shaving • Wire-drawing • Patenting • Rolling • Oil tempering • Eddy Testing
for products satisfying the most demanding specifications. A 150-micron thick layer is shaved off the rod surface to reduce surface defects, remove decarburization and eliminate harmful effects of the wire rod manufacturing process.